What causes weld porosity?
Trapped gas, usually from dirty metal or bad shielding
AMES, Iowa — Weld porosity is gas trapped in the weld metal as it freezes, leaving pinholes or small cavities. The usual causes are contaminated metal, lost or insufficient shielding gas, wet or damaged consumables, a bad technique, or coatings that vaporize in the arc. Porosity weakens a weld and can leak in tanks and pipes. Fixing it usually means fixing the setup, not tweaking the machine.
Dirty or coated metal
Oil, grease, paint, rust, moisture, mill scale and zinc coating release gas when heated. That gas bubbles through the puddle and leaves pores behind. Clean to bright metal before welding, wipe with a residue-free solvent, and remove coatings back from the joint. Galvanized steel is a frequent cause and also makes harmful fumes. Moisture is easy to miss: cold steel that sweats in a warm shop can bring water to the joint, so warm and dry it first.
Shielding gas problems
With MIG and TIG, gas protects the puddle. Wind, drafts and fans can blow it away, and a fan aimed at the weld is a classic mistake. Check the gas flow rate against your machine's recommendations, and look for leaks in hoses, fittings and the regulator. A soapy water test shows leaks. Clean the nozzle of spatter, since a clogged nozzle disrupts the gas flow. Hold the gun at a good angle and keep stickout reasonable. An empty cylinder will also cause sudden, spectacular porosity.
Wet or damaged consumables
Low-hydrogen stick rods like 7018 absorb moisture from the air and need dry storage per the manufacturer. Solid and flux-core wire that has rusted or been stored in a damp shed can cause porosity. Check the wire and rods, and replace anything rusted, damp or damaged. Flux-core wire needs the right polarity and settings to produce its shielding.
Technique and settings
Too long an arc, excessive voltage, a very fast travel speed, a poor ground and wrong gun angle can all let air into the weld zone. Hold a short arc, steady speed and proper stickout, and keep the ground clamp on clean metal. In stick welding, a long arc lets air in and causes pits. If porosity appears only at the start of beads, check your start technique and gas preflow.
Equipment checks
Inspect the gun liner, contact tip and drive rolls, since erratic wire feed disturbs the arc. Check the ground cable and connections. If you have a gas solenoid problem or a regulator that sticks, gas delivery will be inconsistent. Run a few test beads on clean scrap to find out whether the metal or the machine is at fault.
Fixing porous welds
Grind out the porous section until you reach sound metal, clean the joint, correct the cause and re-weld. Don't weld over porosity. For pressure parts, tanks or critical structures, have the work reviewed by a qualified welder.
Quick diagnosis checklist
- Is the metal bright and dry?
- Is the gas flowing at the right rate with no leaks?
- Is there any wind or draft?
- Are rods or wire dry and clean?
- Is the arc length and stickout right?
For related safety and shop information, see the OSHA agriculture page, extension.org and extension.unl.edu. Chase the cause in that order and porosity usually gives up quickly.